Page 141 - 机械工程材料2025年第三期
P. 141
张泽晨,等: S355NL钢风电法兰锻件低温冲击韧性不良的原因
参考文献: [9] ZHOU J,MA D S,CHI H X,et al. Microstructure and
properties of hot working die steel H13MOD[J]. Journal
[1] 戈文英. 风电塔筒法兰用S355NL钢的低温冲击韧
of Iron and Steel Research,International,2013,20(9):
性[J]. 特殊钢,2015,36(5):47-50.
117-125.
GE W Y. Low temperature impact toughness of steel
[10] 周惠久,黄明志. 金属材料强度学[M]. 北京:科学出
S355NL for wind power tower flange[J]. Special Steel,
版社,1989:63-67.
2015,36(5):47-50.
ZHOU H J,HUANG M Z. Strength of metal
[2] 隋红霞,傅程. 低温型风力发电机组设计及认证要
materials[M]. Beijing:Science Press,1989:63-67.
求[J]. 中国船检,2012(5):75-77.
[11] 王磊. 材料的力学性能[M]. 4版. 北京:化学工业出版
SUI H X,FU C. Design and certification requirements
社,2022:159-160.
of low temperature wind turbine[J]. China Ship Survey,
WANG L. Mechanical properties of materials[M].
2012(5):75-77.
4th ed. Beijing:Chemical Industry Press,2022:159-160.
[3] 马洪川. 典型F/B双相钢低温断裂韧性及裂纹扩展行
[12] HOFFMAN A K,UMRETIYA R V,CRAWFORD
为研究[D]. 西安:长安大学,2022.
C,et al. The relationship between grain size distribution
MA H C. Research on low temperature fracture
and ductile to brittle transition temperature in FeCrAl
toughness and crack propagation behavior of typical F/B
alloys[J]. Materials Letters,2023,331:133427.
dual-phase steels[D]. Xi'an:Changan University,2022.
[13] 胡光立, 谢希文. 钢的热处理:原理和工艺[M]. 5版. 西
[4] 张志慧,金涛,马立新,等. Q355C热轧H型钢低温冲
安:西北工业大学出版社,2016:32-35.
击性能不合格的原因分析与对策[J]. 热加工工艺,
HU G L,XIE X W. Heat treatment of steel:Principle
2020,49(13):156-158.
and technology[M]. 5th ed. Xi'an:Northwestern
ZHANG Z H,JIN T,MA L X,et al. Cause analysis and
Polytechnical University Press,2016:32-35.
countermeasures of non-conformity of low-temperature
[14] 许天旱,罗皓荣. U165超高强度钻杆钢韧脆转变临界
impact properties of Q355C hot-rolled H-beam steel[J].
点的表征方法[J]. 材料热处理学报,2022,43(8):125-
Hot Working Technology,2020,49(13):156-158.
[5] 陈一满, 卢爱凤. S355 NL钢低温冲击韧度不合格原因 132.
XU T H,LUO H R. Characterization method of ductile-
分析[J]. 理化检验-物理分册,2017,53(1):73-76.
CHEN Y M,LU A F. Cause analysis of low- to-brittle transition critical point of U165 ultra-high
strength drill pipe steel[J]. Transactions of Materials
temperature impact toughness disqualification of S355NL
steel[J]. Physical Testing and Chemical Analysis Part A: and Heat Treatment,2022,43(8):125-132.
[15] 段贺. 低温用高强度管线钢的组织控制及强韧化机理
Physical Testing,2017,53(1):73-76.
[6] 何春静,庞庆海,李洁,等. 模拟正火温度对Q355E钢 研究[D]. 合肥:中国科学技术大学,2022:38.
锻件组织和性能的影响[J]. 金属热处理,2022,47(6): DUAN H. Study on microstructure control and
123-127. strengthening & toughening mechanism of high strength
pipeline steel for low temperature application [D]. Hefei:
HE C J,PANG Q H,LI J,et al. Effect of simulated
University of Science and Technology of China,2022:
normalizing temperature on microstructure and properties
of Q355 E steel forgings[J]. Heat Treatment of Metals, 38.
2022,47(6):123-127. [16] DUAN H,SHAN Y Y,YANG K,et al. Effect
[7] 马林,张德勇,李伟,等. 厚规格正火轧制Q355NE钢 of microstructure and crystallographic orientation
板低温冲击性能研究[J]. 焊管,2023,46(9):49-52. characteristics on low temperature toughness and fracture
MA L,ZHANG D Y,LI W,et al. Low temperature behavior of pipeline steels[J]. Journal of Materials
impact properties of thick normalized rolling Q355NE Research and Technology,2022,17:3172-3185.
steel plate[J]. Welded Pipe and Tube,2023,46(9):49- [17] LIU M M,LIU Y L,LI H. Deformation mechanism of
52. ferrite in a low carbon Al-killed steel:Slip behavior,grain
[8] 李友彬. Q345E钢低温冲击性能不合格原因 [J]. 理化 boundary evolution and GND development[J]. Materials
检验-物理分册,2023,59(5):34-36. Science and Engineering:A,2022,842:143093.
LI Y B. Reasons for unqualified low temperature impact [18] ZHANG Y H,GUO X C,FU B G,et al. Microstructure
properties of Q345E steel[J]. Physical Testing and and low-temperature impact fracture behavior of
Chemical Analysis Part A:Physical Testing,2023,59(5): QT400-18AL containing Ni[J]. Materials Science and
34-36. Engineering:A,2023,880:145327.
133