Advanced Search
    SONG Wei, WEI Bo, XIAO Hong-jun, LIU Zheng, JIANG Zhuo-jun. Microstructures and Mechanical Properties of Butt Joint of Dissimilar Steels 15Ni3CrMoV and 10Ni5CrMoV[J]. Materials and Mechanical Engineering, 2017, 41(3): 7-12. DOI: 10.11973/jxgccl201703002
    Citation: SONG Wei, WEI Bo, XIAO Hong-jun, LIU Zheng, JIANG Zhuo-jun. Microstructures and Mechanical Properties of Butt Joint of Dissimilar Steels 15Ni3CrMoV and 10Ni5CrMoV[J]. Materials and Mechanical Engineering, 2017, 41(3): 7-12. DOI: 10.11973/jxgccl201703002

    Microstructures and Mechanical Properties of Butt Joint of Dissimilar Steels 15Ni3CrMoV and 10Ni5CrMoV

    • Butt welding was carried out on 15Ni3CrMoV steel and 10Ni5CrMoV steel by TIG(tungsten inert gas) welding and manual arc welding, the microstructure, tensile property, impact property and hardness of the butt joint were studied. The results show that typical dendrite microstructure was found in the weld seam of dissimilar steels butt joint, the grains in weld seam of manual arc welding butt joint exhibit the characteristic of vertical growth, while the grains in weld seam of pulse TIG welding butt joint exhibit the characteristic of horizontal growth. Tensile fracture position of the butt joint at room temperature located in weld seam zone, and the hardness of heat-affected zone is highest. Compared with manual arc welding butt joint, the pulse TIG welding butt joint has higher tensile strength and impact toughness.
    • loading

    Catalog

      Turn off MathJax
      Article Contents

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return