BAI Qiang, YU Li-qiang, SHANGGUAN Feng-shou, MA Yue-peng, LIU Qiang. Causes of Hot-Rolled Cracks Generation in N80Q Oil Casing[J]. Materials and Mechanical Engineering, 2013, 37(9): 100-102.
Citation: BAI Qiang, YU Li-qiang, SHANGGUAN Feng-shou, MA Yue-peng, LIU Qiang. Causes of Hot-Rolled Cracks Generation in N80Q Oil Casing[J]. Materials and Mechanical Engineering, 2013, 37(9): 100-102.

Causes of Hot-Rolled Cracks Generation in N80Q Oil Casing

More Information
  • Received Date: February 06, 2013
  • Macro and micro morphology of cracks in the end of the N80Q oil casing were observed and the mechanical properties and chemical composition of the oil caing were analysed, and the causes of cracks generation were found. The results show that the cracks generated during perforation and hot rolling, and the reasons of cracks generation were the unqualified hot rolling process and nonumiform heating temperature for tube blank.
  • [1]
    赵志毅, 谢建新, 洪慧平.钢管热连轧过程横断面壁厚变化的三维有限元模拟[J].塑性工程学报, 2009, 16(2): 109-112.
    [2]
    杨进能.石油套管裂纹分析[J].金属材料与冶金工程, 2008, 36(2): 37-43.
    [3]
    罗家华.40Mn2V石油套管外折裂纹分析[J].湖南冶金, 2006, 34(6): 18-20.
    [4]
    朱安莉, 王贵成.热轧穿孔内裂纹缺陷分析[J].机械工程与自动化, 2005(1): 45-47.
    [5]
    李连诗.钢管塑性变形原理;M].北京: 冶金工业出版社, 1985: 114-116.

Catalog

    Article views PDF downloads Cited by()

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return