    HE Wen-wu, LIU Jian-sheng, GUO Yin-fang, CHEN Hui-qin, GUO Hui-guang. Grain Growth Behavior of Mn18Cr18N Retaining Ring Steel during Multi-heating Hot Forging Process[J]. Materials and Mechanical Engineering, 2010, 34(7): 20-22.
    Citation: HE Wen-wu, LIU Jian-sheng, GUO Yin-fang, CHEN Hui-qin, GUO Hui-guang. Grain Growth Behavior of Mn18Cr18N Retaining Ring Steel during Multi-heating Hot Forging Process[J]. Materials and Mechanical Engineering, 2010, 34(7): 20-22.

    Grain Growth Behavior of Mn18Cr18N Retaining Ring Steel during Multi-heating Hot Forging Process

    • In order to solve the problem of grain growth for the Mn18Cr18N retaining ring steel during the multi-heating hot forging process,the effect of heating condition on grain size was investigated.The two-heating forging test had also been verified with small samples.The results show that the grain size of forgings had a certain hereditary,and the grain size didn′t dramatically grow when the forging reheated at 1 100℃ for less than 5 h or 1 050℃ for longer time.And the grain growth mode of the steel was D5.9t-D5.90=2.2×1026exp-486 809强激光与粒子束RT·t.
    • loading

    Catalog

      Turn off MathJax
      Article Contents

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return