Advanced Search

    column
    Present Research Situation and Development Trend of the Polymer-based Damping Materials
    TIAN Nong, XUE Zhong-min, FANG Xiao-min, ZHANG Zuo-guang
    2009, 33(6): 1-5.
    Abstract PDF
    Microstructure Evolution in a Nickel-base Single Crystal Superalloy with [110]Orientation during Creep Process
    SHUI Li, YANG Yan-hong, YU Jin-jiang
    2009, 33(6): 6-9.
    Abstract PDF
    Effect of Temperature on Stress Corrosion Cracking Behavior of X70 Pipeline Steel in Alkali Solution
    ZHANG Liang, LI Xiao-gang, DU Cui-wei, FANG Wei
    2009, 33(6): 10-13.
    Abstract PDF
    Distribution of Nano-particles in Nano-Al2O3/Ni Composite Coatings Prepared by Electrophoretic-electrochemical Deposition
    TIAN Hai-yan, ZHU Di, QU Ning-song, ZHU Zeng-wei
    2009, 33(6): 14-17.
    Abstract PDF
    Influence of Magnetic Field Intensities on Microstructure of Al-5%Mn Alloy
    ZHANG Wei-ping, DOU Yong-xiang
    2009, 33(6): 18-21.
    Abstract PDF
    Influence of Surface Roughness of Substrates on Microstructure and Properties of Nano Composite Coatings
    ZHOU Xi-ying, YAN Min-jie
    2009, 33(6): 22-24.
    Abstract PDF
    Dynamic Recrystallization Behavior of Cu-Ni-Si Alloy for Integrated Circuit Materials
    FAN Li, LIU Ping, JIA Shu-guo, CHEN Shao-hua, YU Zhi-sheng
    2009, 33(6): 25-28.
    Abstract PDF
    Effect of Deformation on Order-disorder Phase Transformation in CuZnAl Alloy during Heating Process
    FAN Ping, MU Yun-chao, YUE Xue-qing
    2009, 33(6): 29-30.
    Abstract PDF
    Relationship of Grinding Textures and Surface Friction Coefficient of Common Steels
    ZHU Shuang-xia, LIU Ying, GUO Ji-lin, LI Xiao-bing
    2009, 33(6): 31-33.
    Abstract PDF
    Corrosion Behavior of X80 Pipeline Steel in Simulated Solution of Ku'erle Soil
    XU Cong-min, SHI Kai, ZHOU Yong, ZHANG Rui-feng, LI Xiao, LU Yan-ling, YAO Ting-zhen
    2009, 33(6): 34-36.
    Abstract PDF
    Influences of Temperature-holding Thickness and Finish Rolling Temperature on Martensite/Austenite Islands in X80 Pipeline Steel
    YI Hai-long, MA Qing-shen, DU Lin-xiu, LIU Xiang-hua, WANG Guo-dong
    2009, 33(6): 37-39.
    Abstract PDF
    Influence of [Si(Al)O4] Polymerization Degree on Solidification of Na+
    SUN Wen-biao, FENG Xiang-peng
    2009, 33(6): 40-44.
    Abstract PDF
    Oriented Cutting (001) and (011) Crystalline Planes of Nickel-base Single Crystal Superalloy
    FANG Jian-feng, TIAN Zhi-ling, YAN Ping, ZHANG Jin-yuan, ZHENG Yi
    2009, 33(6): 45-47.
    Abstract PDF
    Comparison of Wet and Hot Aging Resistance of T700 and T300 Carbon Fiber Strengthened Epoxy Resin Composites
    YU Zhi-guo, YANG Sheng-chun, SONG Bi-feng
    2009, 33(6): 48-51.
    Abstract PDF
    Effect of Preheating on Cell-structure of Al Alloy Foam Prepared by Two-step Foaming Method
    CHU Xu-ming, WANG Hui, DAI Ge, ZHANG Yong-ming, HE Si-yuan, HE De-ping
    2009, 33(6): 52-54.
    Abstract PDF
    Preparing Al-20%Sn Alloy by Mechanical Alloying Combining Cold Compacting and Sintering
    LIU Xin, ZENG Mei-qin, MA Ying, ZHU Min
    2009, 33(6): 55-58.
    Abstract PDF
    Microstructure and Mechanical Properties of Mg-4%Al-0.8%Sb-xRE Magnesium Alloy
    WANG She-bin, WANG Shuai, LI Xiao-bin, FAN Jin-ping, XU Bing-she
    2009, 33(6): 59-63.
    Abstract PDF
    Indentation Property of Closed-cell Aluminum Foam under the Flat-end Cylindrical Indenter
    WANG Xin-zhu, WU Lin-zhi, WANG Shi-xun
    2009, 33(6): 64-68.
    Abstract PDF
    Effect of SiC Content and Hot Press Sintering Temperature on Thermal Conductivity Property of AlN-SiC Composites
    CHENG Wei-hua, LI Xiao-yun, QIU Tai, JIA Miao-lei, GAO Yu-han
    2009, 33(6): 69-71.
    Abstract PDF
    Properties of Low Yield Point Steels Used for Earthquake Resistant Buildings
    WEN Dong-hui, SONG Feng-ming, LI Zi-gang, QU Zhao-xia, LIU Zi-cheng, SUN Fei-fei
    2009, 33(6): 72-74.
    Abstract PDF
    Effects of Drying Temperature on Phase Compositions and Properties of Mechanical Galvanizing Coatings
    WANG Sheng-min, SHI Qing-nan, ZHAO Xiao-jun, HE Ming-yi, PENG Zeng-hua
    2009, 33(6): 75-76.
    Abstract PDF
    Microstructure and Depth of Harden Layer of 40Cr Steel Melting Treated with Different Lasers
    LI Gang, QIU Ling, QIU Xing-wu
    2009, 33(6): 77-80.
    Abstract PDF
    Effect of Cr Particle Size on the Oxidation in Air and Hot-corrosion Resistance in Molten Na2SO4 Salt of Ni-Cr Composite Coatings at 900℃
    ZHOU Yue-bo, ZHAO Guo-gang, ZHANG Hai-jun
    2009, 33(6): 81-84.
    Abstract PDF
    Detonation Spraying Cr3C2-NiCr Coatings and Its Effect on Fatigue Property of 2Cr10MoVNbN Steel Substrate
    CHEN Zhao-yun, MENG Xiang-hong, LI Jian-ming
    2009, 33(6): 85-89.
    Abstract PDF
    Friction and Wear Properties of CuTeSeFe Alloy under Dry Sliding Condition
    XUE Yun
    2009, 33(6): 90-92.
    Abstract PDF
    Effect of Heat Treatment Temperature on Microstructure and Hardness of High Vanadium High Speed Steel
    LI Ping, DU Zhong-ze, FU Han-guang, FENG Zhen-jun
    2009, 33(6): 93-95.
    Abstract PDF
    Failure Analysis of Surface Coatings on Furnace Rolls in Annealing Line
    SHI Jian-hua, ZHAO Chun-tao, PENG Xiao
    2009, 33(6): 96-100.
    Abstract PDF